Reference price US$0.05 – 1.20 / m FOB Xiamen · varies with width and order quantity
  • Model No: vc-068

  • Specifications

    Width : 10-150 mm, slit to order (+/-0.5 mm)
    Material : Woven hook and loop
    Colour : Natural / made to order
    Minimum order : 500 m (stock colour) / 3,000 m (dyed)
    Sample : 7 days, cut to width
    Production : 2-3 weeks after sample approval
    Certification : SGS / Oeko-Tex / ISO 9001; REACH and RoHS declarations
    Packing : Polybag, export carton, palletised for LCL
    Port : EXW Xiamen, FOB or CIF
    Payment : T/T 30% deposit, balance against copy of B/L
    Slitting tolerance : ±0.5 mm
  • Inquiry now

Detailed description

If the last shipment had edges fraying, a width that measured wide on arrival, or a peel that read low in incoming inspection, the cause is almost always in one of the four items described on this page rather than in the price.

What the buyer is choosing

Grade and backing are separate decisions. The same woven face is supplied plain for stitching, coated with acrylic for panels, or coated with rubber for rough and low-energy surfaces. Buying the face and the backing as one item is what produces the 'it stuck for a week then fell off' complaint.

The material question

The construction is a woven hook and loop face in the standard grade: enough hook density for a normal closure, priced for volume rather than for a five-year service life. If the application cycles more than a few thousand times, ask for the higher-density weave instead of paying twice for the same part.

How it is quoted

Widths are slit from the master roll in one millimetre steps between 10 mm and 150 mm, held to plus or minus 0.5 mm. A width that is not on the list is a slitting instruction, not a new tool, so it does not add lead time once the master exists.

What ships with the goods

Peel and width are measured on the production lot, not on a sample kept from an earlier run. If your incoming inspection uses a different pull speed or dwell time, tell us and we will match it so the two numbers can be compared.

Checking it on arrival

Do the peel test on the material you will actually bond to, not on a steel plate. The number in the specification is a reference value measured on steel; on powder coat or on a textile it will read differently, and that difference is the one your customer will notice.

Send the grade, width and colour with the annual volume and the quote comes back against a real construction rather than a catalogue range.