Polyester Hook and Loop for Raincoats
Polyester Hook and Loop for Raincoats Thumb

Polyester Hook and Loop for Raincoats

  • Model No: vc-039

  • Specifications

    Width : 10-150 mm, slit to order (+/-0.5 mm)
    Material : 100% Polyester
    Colour : Natural / made to order
    Minimum order : 500 m (stock colour) / 3,000 m (dyed)
    Sample : 7 days, cut to width
    Production : 15-25 days after sample approval
    Certification : SGS / Oeko-Tex / ISO 9001; REACH and RoHS declarations
    Packing : Polybag, export carton, palletised for LCL
    Port : EXW Xiamen, FOB or CIF
    Payment : T/T 30% deposit, balance against copy of B/L
  • Inquiry now

Detailed description

This is a woven hook and loop construction supplied to order. What follows is the part that decides whether the roll works on your line: the yarn, the width tolerance, the put-up and the paperwork that travels with the container.

What the buyer is choosing

Colour is a specification, not a preference. Dyed lots are matched to a retained standard under D65 light, and a black that matches in an office can read green in daylight. If the colour is customer-facing, approve a physical swatch and keep it, because a photograph is not a standard.

The material question

The fibre is polyester. It takes up less water than nylon, so the width is stable in humid storage and in a container crossing the tropics, and it holds up under UV where nylon would chalk. The trade-off is a slightly stiffer hand and a narrower colour range at the deep end.

How it is quoted

Samples ship in seven days, cut to the width you ask for, with the lot report from the run they came from. Bulk runs fifteen to twenty-five days after sample approval, EXW Xiamen, FOB or CIF as you prefer.

What ships with the goods

Packing is poly bag plus export carton, palletised for LCL. For humid destinations we add a desiccant and a moisture barrier, because a roll that takes up water in transit will measure wide on arrival.

Checking it on arrival

On arrival, measure the width at the core and at the outside of the roll before you cut anything. A roll that measures wide at one end and nominal at the other was slit under uneven tension, and the whole lot will behave the same way on your line.

If the grade is still open, send the application and the cycle count and we will tell you which of the three constructions is the cheapest one that will survive it.