Lightweight Black Sticky-Back Nylon Loop Fabric
Lightweight Black Sticky-Back Nylon Loop Fabric Thumb

Lightweight Black Sticky-Back Nylon Loop Fabric

Reference price US$0.05 – 1.20 / m FOB Xiamen · varies with width and order quantity
  • Model No: vc-288

  • Specifications

    Width : 10-150 mm, slit to order (+/-0.5 mm)
    Material : 100% Nylon
    Colour : Black
    Minimum order : 500 m (stock colour) / 3,000 m (dyed)
    Sample : 7 days, cut to width
    Production : 2-3 weeks after sample approval
    Certification : SGS / Oeko-Tex / ISO 9001; REACH and RoHS declarations
    Packing : Polybag, export carton, palletised for LCL
    Port : EXW Xiamen, FOB or CIF
    Payment : T/T 30% deposit, balance against copy of B/L
    Slitting tolerance : ±0.5 mm
  • Inquiry now

Detailed description

Most enquiries for this item come down to three decisions made in the wrong order: grade, width, then price. Grade sets the cycle life, width sets the roll cost, and the unit price is only comparable once the first two are fixed.

What the buyer is choosing

Grade and backing are separate decisions. The same woven face is supplied plain for stitching, coated with acrylic for panels, or coated with rubber for rough and low-energy surfaces. Buying the face and the backing as one item is what produces the 'it stuck for a week then fell off' complaint.

The material question

The fibre is nylon (polyamide). It takes dye deeply, which is why the colour range is wide and why the colour holds through washing at 40 degrees. Its weakness is moisture regain: a nylon roll absorbs water in transit, measures wide on arrival and settles back over about a week, so allow for it in incoming inspection rather than rejecting the lot.

With the liner-backed version, position the part before exposing the adhesive and roll it down with firm pressure. A peel test run twenty minutes after application reads low by design and should not be used to reject a lot.

How it is quoted

Samples ship in seven days, cut to the width you ask for, with the lot report from the run they came from. Bulk runs fifteen to twenty-five days after sample approval, EXW Xiamen, FOB or CIF as you prefer.

What ships with the goods

Colour is checked against the retained standard under D65 on every lot, and weft skew, oil marks and hook damage are inspected across the full roll rather than on a cut sample.

Checking it on arrival

Do the peel test on the material you will actually bond to, not on a steel plate. The number in the specification is a reference value measured on steel; on powder coat or on a textile it will read differently, and that difference is the one your customer will notice.